This does not sound like thermal polymerization to me, but rather like
radical formation by cosmic rays, light, oxygen or the like. But I am no
expert either.
Oliver 'Ojo' Bedford <newsojo@xxxxxx> schrieb in im Newsbeitrag:
dqb5v7$so5$1@xxxxxxxxxxxxxxxxxxxxxxxxxxxxx
> In our lab we had a styrene bottle which had polymerised in the
> fridge. So, I would conclude the upper limit lies below 4 °C.
>
> Regards,
> Oliver
>
.