Re: polyurethane composite bubble problem



mingzong@xxxxxxxxx wrote:
> hi, I am doing a projectof polyurethane-glass fiber composite.
> Although I dryed the glass fiber before it was used, however, when I
> transfer the glass fiber from the oven to the processing machine, it
> absorbs water. The water absorbed by glass fiber react with PU and
> produce bubble in the composite. Does any one know how to get rid of
> the water in the composite? Thanks.

Hopper mounted drying system. -40DP minimum (Desiccant, CDA, Vacuum).
Another way you can go is nitrogen purge on your hopper.


.



Relevant Pages

  • polyurethane composite bubble problem
    ... I am doing a projectof polyurethane-glass fiber composite. ... I dryed the glass fiber before it was used, however, when I transfer ... The water absorbed by glass fiber react with PU and produce ...
    (sci.polymers)
  • Re: polyurethane composite bubble problem
    ... You might have water in your resin to start with in which case a moisture ... >> I dryed the glass fiber before it was used, however, when I transfer ... > a high temperature oven to a significantly lower temperature area quickly? ...
    (sci.polymers)