- From: Steve <steve@xxxxxxxxxxxxxx>
- Date: Wed, 18 Jan 2006 19:11:27 +0000
ricarrios@xxxxxxxxx wrote:
Dear friends
I have recently heard that it is not appropriate to cut steel with diamond wheels, because the high wear of the cutting wheel.
True.
Steve .