Re: Stick or MIG ?



On Thu, 3 May 2012 17:49:13 -0500, "Snag" <snag_one@xxxxxxxxxxx> wrote:

I just got an order for another AC cage , and since the tombstone is up
and running now I'm considering using it for this one . I used the Weldpak
100 for the last one and felt it was just barely up to the task . I'll be
using 11ga 3/4" square tube , and have on hand 6011 , 6013 , and 7018 in
1/8" for the stick welder - and I can get some 3/32" in those 3 locally . I
have .035" flux core and .025" ER70S6 with CO2 or C25 for the MIG .

Which would y'all use ?

3/32 6011 or 6013. Or good .035 with CO2 for mig. CO2 really adds a
fair amount of heat. You CAN use .35 flux core with gas..but its kinda
a waste in most cases like this.

Ive got about 5 tanks of C25..and use them very very seldom. I depend on
C02 for most of my welding, which is rough duty.

Gunner

--
"The danger to America is not Barack Obama but a citizenry
capable of entrusting a man like him with the Presidency.
It will be far easier to limit and undo the follies of an
Obama presidency than to restore the necessary common sense
and good judgment to a depraved electorate willing to have
such a man for their? president.. Blaming the prince of the
fools should not blind anyone to the vast confederacy of
fools that made him their prince".
.



Relevant Pages

  • Re: Whats With This So-Called "Old Guy?"
    ... He worked long and hard to make a good life only to have ... "The danger to America is not Barack Obama, but a citizenry capable of entrusting a man like him with the Presidency. ... It will be far easier to limit and undo the follies of an Obama presidency than to restore the necessary common sense and good judgment to a depraved electorate willing to have such a man for their president. ... Blaming the prince of the fools should not blind anyone to the vast confederacy of fools that made him their prince. ...
    (rec.outdoors.rv-travel)
  • Re: Whats With This So-Called "Old Guy?"
    ... He worked long and hard to make a good life only to have ... entrusting a man like him with the Presidency. ... anyone to the vast confederacy of fools that made him their prince. ... Republic can survive a Barack Obama, who is, after all, merely a fool. ...
    (rec.outdoors.rv-travel)
  • Re: And The Fools Have Elected Their Prince
    ... "The danger to America is not Barack Obama, ... entrusting a man like him with the Presidency. ... anyone to the vast confederacy of fools that made him their prince. ...
    (alt.religion.christian.roman-catholic)
  • Re: O/T: Major Sea Changes
    ... "The danger to America is not Barack Obama but a citizenry capable of ... entrusting a man like him with the Presidency. ... Blaming the prince of the fools ...
    (rec.woodworking)
  • a citizenry capable of entrusting a man like him with the Presidency
    ... "The danger to America is not Barack Obama, but a citizenry capable of entrusting a man like him with the Presidency. ... It will be far easier to limit and undo the follies of an Obama presidency than to restore the necessary common sense and good judgment to a depraved electorate willing to have such a man for their president. ... Blaming the prince of the fools should not blind anyone to the vast confederacy of fools that made him their prince. ...
    (alt.politics)