Re: Stick or MIG ?
- From: Glenn Lyford <glyford@xxxxxxxxx>
- Date: Fri, 4 May 2012 06:22:49 -0700 (PDT)
On Thursday, May 3, 2012 6:49:13 PM UTC-4, Snag wrote:
I'll be
using 11ga 3/4" square tube , and have on hand 6011 , 6013 , and 7018 in
1/8" for the stick welder - and I can get some 3/32" in those 3 locally . I
have .035" flux core and .025" ER70S6 with CO2 or C25 for the MIG .
Which would y'all use ?
I'd use 3/32 in either 7014 or 7018, but since you have 1/8 on hand I'd try that first. I have not had great luck getting 60xx rods to run well, but if you have no problems with that then any of the rods you list should work.
I've not played with MIG, so I'll let someone else answer that part.
.
- Follow-Ups:
- Re: Stick or MIG ?
- From: Snag
- Re: Stick or MIG ?
- References:
- Stick or MIG ?
- From: Snag
- Stick or MIG ?
- Prev by Date: Re: Hardfacing
- Next by Date: Re: Hardfacing
- Previous by thread: Stick or MIG ?
- Next by thread: Re: Stick or MIG ?
- Index(es):