Re: Crappy bead w/ Miller Spoolmatic 30A



Oops!
for Nogas Nozzle, read Gas Nozzle!
(Freudian slip!)

"Potblak" <Invalid@xxxxxxxxxxx> wrote in message
news:44f3de5a$0$10763$5a62ac22@xxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxx
Sounds like the Argon isn't reaching the nogas nozzle or is heavily
contaminated.
Have you;
1. checked for leaks?
2. measured the gas flow at the gun?

The soot either side of the bead is actually carbon deposit from decomp of
grease either on the wire or the job, and actually indicates at least some
gas is getting through.

What arc voltage and current are you running at?
A rule of thumb is Arc Volts=14+(Amps/20)

<Sierevello@xxxxxxx> wrote in message
news:1156826908.375968.59940@xxxxxxxxxxxxxxxxxxxxxxxxxxxxxxx
I tried tacking some ears onto a Muncie transmission with my Spoolmatic
30A that is running off my Millermatic 250/ meters mig. I meticulously
cleaned both the tranmission and also the 6061-T6 ears. I have had the
gun for a year and just decided to hook it up. Gun is positive as per
the directions and ground is negative. 20cfh on the argon and a roll of
4043 in .035". Tip is correct and ground was good and I gave a
substantial preflow of argon before striking the arc. Gun at about 10
degees from veritcal and pushing.

Lots of smoke and a bead that looked like Mount St. Helens. Zero
penetration and a black soot on each side of the weld bead. The gun was
set as per the specs for 1/4" aluminum. The transmission is 365
aluminum and is quite weldable. The gas is good because it is the same
bottle I run off of my TIG machine.

I then tried it on an old scrap transmission after cleaning it also. I
got the same results.

Anybody have any idea what is going on here?

Any help or tips greatly appreciated.

Thanks, Steve





.



Relevant Pages

  • Re: Crappy bead w/ Miller Spoolmatic 30A
    ... It sounds like you may have gotten some cheap recycled aluminum, ... for Nogas Nozzle, read Gas Nozzle! ... gun for a year and just decided to hook it up. ...
    (sci.engr.joining.welding)
  • Re: Musing about muzzleloaders
    ... Windage could have been abolished with artillery much earlier than it actually was. ... The trouble was that windage not only made loading easier it kept internal pressure down to a safe level. ... Built up artillery allowed variations in gun strength to allow for the pressure curve along the barrel. ... Combined with chambering to allow initial gas expansion it made it worthwhile reducing windage. ...
    (sci.military.naval)
  • Re: OT: Stranger on my front porch at 4:00 am
    ... I opened the door after getting my gun & the guy is ... in a bind & needed Gas. ... guy or just shoot him in the damn foot, But at 4:00 am I'm not in the ... mood for shit like this, I figured if I shot him in the foot, I'd be ...
    (rec.games.pinball)
  • Re: Requirement for licensing a laboratory gas gun?
    ... in mass (including compressed gas tanks), ... it sounds like a shot gun licence is required. ... It includes any prohibited weapon, ... muzzle energy being over 12 ftlbs, would qualify as a firearm. ...
    (uk.legal)
  • Re: OT: Stranger on my front porch at 4:00 am
    ... I opened the door after getting my gun & the guy is ... in a bind & needed Gas. ... guy or just shoot him in the damn foot, But at 4:00 am I'm not in the ... mood for shit like this, I figured if I shot him in the foot, I'd be ...
    (rec.games.pinball)