Plasma Cutters..



Over and over this group reccomends the Thermal Dynamics Plasma cutters.

I was about to purchase a Thermal Dynamics Cutmaster 51,
alas as I was searching for the best price I found the

Thermal Dynamics Drag Gun Plus....
Looks like similar specs with the built in air compressor...

Other units with the built in air compressors
have looked like toys, alas this one claims to do
a quality cut on 1/2" (13mm) steel.

Does anyone have any experience with this?
If the two units are close in perfromance the
hassle reduction of not having to run an air hose would
be worth some minor loss in capability.
this is for serious hobby use, not industrial fabrication.\


Paul
.



Relevant Pages

  • Re: Plasma Cutters..
    ... Over and over this group reccomends the Thermal Dynamics Plasma cutters. ... alas as I was searching for the best price I found the ... Looks like similar specs with the built in air compressor... ...
    (sci.engr.joining.welding)
  • Re: Plasma Cutters..
    ... I got thermal dynamics and hyper therm confused.... ... The choices are Hypertherm Power max 600 vs the drag gun plus... ... Looks like similar specs with the built in air compressor... ...
    (sci.engr.joining.welding)