Re: welding aluminum with deca 135e



I'm totally amazed you can weld anything at all with it!
"Chris" <doomroom@xxxxxxxxxxxxxx> wrote in message
news:ohveg.2089$ou6.1949@xxxxxxxxxxxxxxx
Hi, all!

I have a deca 135e wirefeed welder. I plan to use it mostly for autobody
and bike frames.
I was having trouble burning holes through 22 guage *** metal, but
thanks to a previous thread, I've switched from
.035 fluxcore to .030 fluxcore with adequate results. I will probably
switch to gas when I can afford to.

There is a teflon liner kit available for aluminum. what results can I
expect from an 55-85A welder on aluminum?
can I weld 1/16" bike tubing with this? or 1/16" to 1/8 bracket?

thanks,
- Chris




.