Re: weight per foot: 4" x 4" x .375" inch angle iron? for 'the monolith' toolbox... (pix too)



9.74 lb/ft sez the table I have.

--
Regards,
Carl Ijames carl.ijames at verizon.net

would some kind soul please provide me the weight per foot info for
this 'fairly large' angle iron? all I know right now is
it's -extraordinarily- heavy.


.