Re: SIP Migmate spares (UK)
- From: Steve Taylor <steve@xxxxxxxxxxxxxxxxxxxxxx>
- Date: Tue, 02 May 2006 11:06:16 +0100
Martin Whybrow wrote:
I'm using a SIP Migmate Pro 170DP Turbo for welding aluminium. I have the
proper Teflon liner in the (Euro) torch but I am getting faltering wire
feeding and occasional poor contact in the tip; looking at the wire, it's
got an embossed pattern on it from the feed roll which has a knurled groove
in the 0.8mm position (using 0.8mm wire). I would like to replace the feed
roll with a proper 'U' groove roll but the manual's spare parts list is a
joke (it simply shows a diagram with the larger items inside the welder) and
has no part numbers; anyone know if a proper parts list exists for the
Migmate, where I could buy a spare feed roll or if it's possible to fit
parts from another make (seeing as these are made in Italy in a factory that
makes at least 2 other brands of MIG)?
TIA, Martin.
SIP are utterly bloody useless - I have been waiting 6 weeks for spare tips for my Plasma cutter - so long, I have decided to turn some of my own up.
Can't you get someone to turn you a suitable roller ?
Steve
.
- Follow-Ups:
- Re: SIP Migmate spares (UK)
- From: Balders
- Re: SIP Migmate spares (UK)
- References:
- SIP Migmate spares (UK)
- From: Martin Whybrow
- SIP Migmate spares (UK)
- Prev by Date: Re: Weird TIG arc instability
- Next by Date: Re: SIP Migmate spares (UK)
- Previous by thread: SIP Migmate spares (UK)
- Next by thread: Re: SIP Migmate spares (UK)
- Index(es):
Relevant Pages
|
Loading