CFM is strictly a function of the orifice size and pressure. Doubling
the psi on your gauge will double the CFM but the exact calibratin
depends on the size of the gas orifice in your machine.
a6016 wrote:
What is the correlation between pressure in pounds per square inch & a
cubic foot measurement? For tig I guess is cubic feet per hour? Gauge
I have is in PSI and everything I see to guide me in setting argon flow
is in cubic feet. TIA.
Vic
Redlands, CA.
.
Relevant Pages
- Re: Micro Air Compressor
... I have a little 12V compressor ... that will produce .3 CFM at 100 psi. ... why *not* a compressed air cylinder? ... (sci.engr.mech) - Re: Which controls do I add to show, edit and save test parameters?
... 'valve open' text boxes like 'CFM' and 'PSI'. ... relational database, just a table or flat file'. ... I would definitely decouple the UI from the storage. ... (microsoft.public.dotnet.languages.csharp) - Re: Which controls do I add to show, edit and save test parameters?
... 'valve open' text boxes like 'CFM' and 'PSI'. ... just a table or flat file'. ... control would let me open the file, edit the cells, and save it back? ... (microsoft.public.dotnet.languages.csharp) - Re: Compressor/tire pressure equalization?
... happen to be set @ 100, which is a decent pressure for my road bike. ... the tire (somewhere between 0 and 100 psi) is proportional to the pressure ... Okay, seems reasonable, with the regulator set at 100 and assuming a ... But where would most roadies carry a gauge? ... (rec.bicycles.tech) - Re: Which controls do I add to show, edit and save test parameters?
... 'valve open' text boxes like 'CFM' and 'PSI'. ... just a table or flat file'. ... control would let me open the file, edit the cells, and save it back? ... (microsoft.public.dotnet.languages.csharp) |
|