Scale is really nasty sometimes. I had a slab of 3/8" IIRC on the table and it was hot rolled - scale thick. The table wouldn't connect. I had to grind a shinny spot and clamp onto the slab myself. (slab is slang :-) ). I later determined that even on nice metal - the work clamp was really a post clamp (a.k.a. Battery charger) and had little contact surface to pass current. I replaced it with a 300 amp that (I don't use 300 but it improves the connection!!) has three rods that clamp on the metal. Easy task. Lower resistance and lower inductance - both killers to DC current and HF arc.
Martin Martin Eastburn @ home at Lions' Lair with our computer lionslair at consolidated dot net NRA LOH, NRA Life NRA Second Amendment Task Force Charter Founder
bob wrote:
cl wrote:
bob wrote:
thanks for the tips, i will try again
What is your powersource (110 or 220) and air comp capacity?
I am plugged into a Generac 4000 xl generator, 230 volts ,4000 watts. I can pull maybe 17 amps out of it (220 v). I could wire the plug 110 if necessary ?. I can pull 30 amps then on 110v. My air compressor is a Ingersol Rand 5 hp, gas engine air compressor, the ones u see with two small tanks but volume is NO PROBLEM, I have 50 feet of air hose going to two air filters. I a pretty sure the air is dry and oil free. But I could be very wrong.
----== Posted via Newsfeeds.Com - Unlimited-Uncensored-Secure Usenet News==---- http://www.newsfeeds.com The #1 Newsgroup Service in the World! 120,000+ Newsgroups ----= East and West-Coast Server Farms - Total Privacy via Encryption =---- .
- References:
- Hypertherm Powermax 380 problems
- From: bob
- Re: Hypertherm Powermax 380 problems
- From: Wayne Cook
- Re: Hypertherm Powermax 380 problems
- From: bob
- Re: Hypertherm Powermax 380 problems
- From: cl
- Re: Hypertherm Powermax 380 problems
- From: bob
- Hypertherm Powermax 380 problems
- Prev by Date: Re: begginers weld problems with OA
- Next by Date: Re: Can I mig weld with pure argon?
- Previous by thread: Re: Hypertherm Powermax 380 problems
- Next by thread: Plasma arc cutting
- Index(es):
Relevant Pages
|