On 29 Aug 2005 20:24:08 -0700, "stag5353" <adamstagnaro@xxxxxxxxx>
wrote:
>Yeah, I was just out there welding and I pointed the torch at a piece
>of scrap and hit the pedal while looking the other way... the lights
>went out completely until I moved the tungsten in and established an
>arc. Voila. Kind of funny cause I could never tell if they were out the
>whole time I was welding...
>
>yep, only the TIG. Seems to be the HF (High Frequency, not Harbor
>Freight, ha ha). I wonder what causes this in the lights???
Sounds like a bad ground path/ground loop. Ground the welder body and
the bench if you have one.
Gunner
.
- References:
- TIG makes my fluorescent lights flicker...
- From: stag5353
- Re: TIG makes my fluorescent lights flicker...
- From: Martin H. Eastburn
- Re: TIG makes my fluorescent lights flicker...
- From: acrobat ants
- Re: TIG makes my fluorescent lights flicker...
- From: stag5353
- TIG makes my fluorescent lights flicker...
- Prev by Date: Re: TIG makes my fluorescent lights flicker...
- Next by Date: Re: "keyhole" shape?
- Previous by thread: Re: TIG makes my fluorescent lights flicker...
- Next by thread: HF is messing with the circuits in the helmet
- Index(es):
Relevant Pages
|