Another trick is to use a cold chisel to raise a sliver on the metal
and heat that to get started. Useful on thick material where getting
the metal red hot takes a long time.
Dan
Leo Lichtman wrote:
>
> One trick to being able to start the cut earlier is to drill a small hole,
> and start cutting as soon as the edge of the hole gets red. This also helps
> when you don't have enough heat--once you get the oxygen to start burning
> the steel, you really don't depend on the preheat, as dcaster and R
> Zimmerman pointed out.
.
- Follow-Ups:
- Re: Cutting advice please
- From: mhorowit
- Re: Cutting advice please
- References:
- Cutting advice please
- From: Michael Horowitz
- Re: Cutting advice please
- From: Leo Lichtman
- Re: Cutting advice please
- From: Michael Horowitz
- Re: Cutting advice please
- From: Leo Lichtman
- Cutting advice please
- Prev by Date: Re: cutting a fishmouth joint
- Next by Date: Re: Critique my weld please
- Previous by thread: Re: Cutting advice please
- Next by thread: Re: Cutting advice please
- Index(es):
Relevant Pages
|