Re: Calling Alvin Johnson...



Thanks! What kind of books should I look for on the topics of
ductility vs hardness as a function of temper in 1075 and that sort of
thing? Like the charts on Cliff's guide to 1095.

.



Relevant Pages

  • Re: Grits of sandpaper to use when finishing a blade.
    ... Got any charts that deal with cold treatment? ... It would have to show the hardness changes with a cold ... Lots of information about cold treating A2, it's a die steel where ... optimum temper to make it really tough and then figure out how much hardness ...
    (rec.knives)
  • Re: Is This A Fossil? (Help Please)
    ... Looks like graphic intergrowth to me in some sort of ... pegmatite, but difficult to say without a hand lens examination. ... hardness like? ...
    (sci.geo.geology)
  • How hard should I make a bowie knife from L6??
    ... and was wondering what sort of hardness I should get them treated too ... No Alvin not 64 rockwell ... They are bowie/clip point knives made from Admiral Steels L6 ...
    (rec.knives)
  • Re: How hard should I make a bowie knife from L6??
    ... IMHO best would be a hardness gradient front to back of approx R60 to R48 ... and was wondering what sort of hardness I should get them treated too ... No Alvin not 64 rockwell ... They are bowie/clip point knives made from Admiral Steels L6 ...
    (rec.knives)
  • Re: D2 hardness
    ... hardness and the edge was 68 rockwell c.  Seems sort of over the top. ... They only show cutting tests, ... I'd like to see how that edge hardness ...