Re: HEAT RETENTIVE PLATES



Bob,
The trick is not only the mass of the heater or susceptor inside the
plate, but
how efficient it is to capture microwave energy very fast and how it
is released at a controlled rate. I capture about 1200 Watts minutes of
energy and release it at the rate of about 37.5 watts per minute, that
is like having a light bulb of 37.5 Watts inside your plate.
Could you post this to all your groups?
I'm new to this. I will really appreciate it.
Juan


Bob Masta wrote:
On 23 Jul 2006 05:51:50 -0700, "steve slgraber@xxxxxxx"
<slgraber@xxxxxxx> wrote:

bob, sounds like a scam to buy his plate. much like a perpetual motion
machine. if a plate retained heat so well, it wouldn't do much good in
keeping steaks warm either.


I don't see him claiming anything that violates any laws of physics.
A plate is a big mass, relative to the food you put on it. If you
put food on a cold plate, the food will cool down faster than if
you put it on a warm plate, because the food is transferring heat
to the plate due to the temperature difference. As I understand
his design, it just reverses the situation so the plate is as hot as
or hotter than the food. As a bonus, the plate apparently has
embedded in it a big slug of some substance that heats up via
microwaves. That extra mass will further extend the temperature
decay time. Nothing tricky about that, it's just like heating
a heavy plate in a conventional oven before you serve the food.
His invention is all about heating it quickly in the microwave,
without cracking the plate.

Best regards,


Bob Masta
dqatechATdaqartaDOTcom

D A Q A R T A
Data AcQuisition And Real-Time Analysis
www.daqarta.com
Home of DaqGen, the FREEWARE signal generator

.



Relevant Pages

  • Re: Sweet Potato Fries
    ... I've always wanted a decent french fry cutter, ... friends is a food cover for use in a microwave oven. ... If anybody uses a microwave oven, this saves one heck of a lot ... Where we use the covers is with food on a plate. ...
    (alt.food.barbecue)
  • Re: (2008-06-16) NS-RFC: Party crashers...
    ... I almost lost it when I watched one of them eat a big plate ... The ones that want to take food home are the worst IMO. ... Tupperware containers, loading stuff up to take home. ...
    (rec.food.cooking)
  • Family Kicked Out of All You Can Eat Buffet Restaurant
    ... Iowa - Wendy Dershem may think twice before ... leaving that egg roll on her plate at her next Chinese buffet. ... "We waste too much food. ...
    (rec.sport.pro-wrestling)
  • Re: (2008-06-16) NS-RFC: Party crashers...
    ... I almost lost it when I watched one of them eat a big plate ... The ones that want to take food home are the worst IMO. ... Tupperware containers, loading stuff up to take home. ...
    (rec.food.cooking)
  • Re: Scary Shows On TLC
    ... money to pay for his fast food order, and then pulled the food back ... plate full of biscuits, a bucket of fried chicken, a plate of ... to improve my adherence to my low-carb diet. ... used to sing "fat songs" to me and those always seemed to keep me on the ...
    (alt.support.diabetes)