On Mar 5, 3:58 pm, t_pas...@xxxxxxxxxxx wrote:

Incidentally, the dealer did tell me about the "Burma" Jade and
supposedly this is Burma Jade, A-grade stuff. I don't know about
nephrite and jadeite, etc., his English wasn't perfect, obviously.
It's white, as I said, with green flakes, purple shadows and the more
I wear it, the more I like it.

From your description it's clearly jadeite and not nephrite.

And thanks to Peter for the elaborations, I think I bought the right
material beads, going for jadeite rather than nephrite.

Maren
HiloBeads: Beads - Beading Supplies - Hand-made Jewelry
http://www.hilobeads.com/
(yes, I know, I shouldn't call that jewelry here, I'm just a bead
person)
.



Relevant Pages

  • OT, thanks to Peter. was: Re: Curious about Jade appraisal
    ... material beads, going for jadeite rather than nephrite. ... quite tough as far as gem materials go. ...
    (rec.crafts.jewelry)
  • Re: Jade versus Jadeite
    ... My mom recently returned from China with a couple of "jadeite" ... There are two distinct minerals that are called Jade. ... with various roiled textures or black spots, and the like, are nephrite jade. ... So while it's entirely possible that your mom got great jade bracelets ...
    (rec.crafts.jewelry)