Re: Gold plating
- From: Abrasha <abrasha@xxxxxxxxxxx>
- Date: Fri, 17 Feb 2006 08:16:43 GMT
mbstevens wrote:
Jack Schmidling wrote:
I was basing it on what I paid for a much smaller quantity of
non-cyanide solution and I agree, cost is not an issue especially if the
gold can be replenished.
The unanswered question is, can I replenish the gold in the non-cyanide
based solution?
I've added a bit of gold to mine successfully. I _suspect_ the
solution is mostly aqua regia.
What is "mostly" Aqua Regia?
Aqua Regia has a very limited life span.
And try plating precious metal in Aqua Regia. Do you know what happens? Look
it up.
--
Abrasha
http://www.abrasha.com
.
- References:
- Gold plating
- From: Jack Schmidling
- Re: Gold plating
- From: Abrasha
- Re: Gold plating
- From: Jack Schmidling
- Re: Gold plating
- From: Abrasha
- Re: Gold plating
- From: Jack Schmidling
- Re: Gold plating
- From: mbstevens
- Gold plating
- Prev by Date: Re: Rolling Mill
- Next by Date: Re: Gold plating
- Previous by thread: Re: Gold plating
- Next by thread: Re: Gold plating
- Index(es):
Relevant Pages
|